Copper leaching-extraction-electrowinning

EPC project profile

Low-grade copper oxide ore, waste copperish ore and other copper-containing materials can be leached and extracted, and copper can be extracted and separated from the leaching solution with low copper concentration and enriched to copper sulfate solution containing about 50g/l of copper. The solution then goes through an electro-winning process to produce 99.99% copper cathode.

EPC contract range:From leaching liquid to cathode copper.